![Sharp Cut Dichroic Mirror Sharp Cut Dichroic Mirror](https://www.optosigma.com/media/catalog/product/cache/b27e9de4b013e3855bcfc3a2fcf2e141/4/7/47644c90fce5c9008a1ea6c216939abfe12c95ff_sdm_p_1.jpg)
In stock
SKU
SDM
Divides sharply the color of wavelength by reflecting the short wavelength and transmitting the long wavelength. Suitable for use in Bio-imaging and flow cytometry applications.
![custom product](https://www.optosigma.com/media/cms/custom-icon.png)
Customize product
Filters
Enabled filters :
Remove all filters
Name | Reflectance | Transmittance | Delivery | Price | Add to cart | |||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
i
Sharp cut dichroic mirror 515nm
SDM515S |
>99% | >avg. 90%/>75% (avg. ; average with respect to wavelength) |
1-3 weeks
|
- |
![]() |
|||||||||||||||||||||||
i
Sharp cut dichroic mirror 455nm
SDM455S |
>99% | >avg. 92%/>avg. 88% (avg. ; average with respect to wavelength) |
1-3 weeks
|
- |
![]() |
|||||||||||||||||||||||
i
Sharp cut dichroic mirror 490nm
SDM490S |
>99% | >avg. 90%/>75% (avg. ; average with respect to wavelength) |
1-3 weeks
|
- |
![]() |
|||||||||||||||||||||||
i
Sharp cut dichroic mirror 570nm
SDM570S |
>99% | >85%/>60% |
1-3 weeks
|
- |
![]() |
|||||||||||||||||||||||
i
Sharp cut dichroic mirror 410nm
SDM410S |
>90%/>99% | >80%/>87% |
1-3 weeks
|
- |
![]() |
|||||||||||||||||||||||
i
Sharp cut dichroic mirror 505nm
SDM505S |
>99% | >85%/>60% |
1-3 weeks
|
- |
![]() |
|||||||||||||||||||||||
i
Sharp cut dichroic mirror 595nm
SDM595S |
>99% | >avg. 92%/>75% (avg. ; average with respect to wavelength) |
1-3 weeks
|
- |
![]() |
You must be logged in to ask questions
◦The short wavelength has high reflectance, fits perfectly for use in excitation light and fluorescence imaging.
◦The feature of the structure of this mirror is to maintain the distance of the edges of the P polarization and the S polarization to be close to each other. It narrows the gap of the reflective range and the transmission range to provide a steep rise.
◦There is limited absorption due to the dielectric coating.
◦The feature of the structure of this mirror is to maintain the distance of the edges of the P polarization and the S polarization to be close to each other. It narrows the gap of the reflective range and the transmission range to provide a steep rise.
◦There is limited absorption due to the dielectric coating.